Medium setting type SM-LM(cationic )
Product specifications:
Name | Asphalt emulsifier SM-LM (cationic ) | |
Test item | Standard | Test result |
Appearance | Creamy white paste or wax | Meet |
Chromaticity(Times)
| 60-100 | 80 |
Content(%) | 80±2 | 80.5 |
Solvent water(%) | 20±2 | 19.5 |
PH value (1% aqueous solution) | 6.5-7.5 | 7.2 |
Water solubility | Soluble and no impurities in room temperature water | Meet |
Features:
1. It has good construction of demulsification which is easy for operate.
2. With the aggregate adhesion of nearly 100%.
3. Emulsification without acid.
Usage:
1. It has excellent compatibility with SBS, the emulsified asphalt can be used for SBS latex modified.
2. Its emulsified asphalt can be applied to the following items:
1) road pavement oil;
2) slurry seal;
3) RAP emulsified asphalt regeneration application;
Reference dosage:
The total amount of the emulsion 0.3-0.4%.Please ask the technician to test for the best dosage according to the asphalt label and brand.